This test method is used to determine the premature failure susceptibility of asphalt mixture due to weakness in the aggregate structure, inadequate binder stiffness, or moisture damage. This test method measures the rut depth and number of passes to failure.
MTI laboratories are accredited by TAF (ISO/IEC 17025) to perform testing standard AASHTO T324 for Hamburg Wheel-Track Testing of Compacted Asphalt Mixtures.